Just the usual Shino...AT Ball Clay 1 : China Clay 1: Nepheline Syenite 1
Someone suggested it was the NS that did it...is there any way I can add something to the glaze to get it to behave? Or do I have to chuck out this batch and start again?
That'll teach me a lesson about testing new batches.....